中文版 | ENGLISHWelcome to our website!

HOTLINE

+86 519 83828901

Chopped Strand Mat

Chopped strand mat is made from fiberglass strands chopped to length and bonded together with powder or Emulsion binder. Chopped strand mat is used primarily for hand lay-up processes, filament winding and press molding of FRP products. Typical products in cluds bathroom accessories, pipe, build in materials, automobiles, furnitures and other FRP products.

Chopped Strand Mat
Chopped strand mat is made from fiberglass strands chopped to length and bonded together with powder or Emulsion binder. Chopped strand mat is used primarily for hand lay-up processes, filament winding and press molding of FRP products. Typical products in cluds bathroom accessories, pipe, build in materials, automobiles, furnitures and other FRP products.

Product Capabilities
Uniform in distribution, without defects of fuzz
Fast and consistent we-out speed in resins
Easily fills mold and conforms to complex shapes

Applications
It is suitable for GFRP products that are formed through pasting by hand or molding. It is wide used for all kinds of products such as automobile, ship body, sanilary ware, electric insulator, anti-corrosive pipe and so on.
The light weight chopped strand mat (100g- 225g) which we supplied possesses high advantages in terms of quality and price.

Technical Specifications

Product code

Component of glass fiber

Width mm

Weight
g/m2

Conpatible Resin

Applying process

Loss on Ignition: %

Moisture content %

Adhesive

EMC

E-glass

250-3200

100-900

Polyester

Hand lay-up

2.0-9.0

=0.2

Powder,
Emulsion

CMC

C-glass

250-3200

100-900

Polyester

Hand lay-up

2.0-9.0

=0.2

Powder,
Emulsion

﹡Specific product properties indicated in quality analysis report. 
 


Packing
Each roll is wound on a cardboard tube(exterior diameter 76mm)and protected by a plastic bag,then be put into a carton.
Rolls can be loaded into a container directly or on pallets.
﹡Special products are according to customer’s requirements.

Storage
Products shalt be placed under dryness condition and the covering membrane shall be no opened until applying.